Flexural Bending Strength Vs Coefficient of Variation

Glass Types Flexural Bending MOR (N/mm2) (MPa) Coefficient of Variation
Annealed Glass 41 0.25
Heat Strengthened Glass 82 0.2
Fully Thermal Tempered Glass 165 0.15
Chemically Strengthened Glass 300 - 600 0.10 - 0.15

Impact Resistant Vs Glass Thickness Vs Ball Drop Height

Impact-Resistant-Vs-Glass-Thickness-Vs-Ball-Drop-Height.png