|  1. When the well-assembled glass with EVA is 
                                loaded, vacuum is started,. 
                                 2. Then it is increased from room temperature 
                                  until the glass surface reaches about 80 oC. 
                                  It is then kept at this temperature for about 
                                  10-30 minutes, depending on glass thickness. 
                                 
                                3. Then, the glass surface is cooled down to 
                                  40 oC. 
                                4. The vacuum is then turned off and the glass 
                                  can be unloaded. 
                                 
                                  Remarks 
                                This process instruction is only for reference. 
                                  The procedure and data are vary depending on, 
                                1. the design and structure of the oven. 
                                  2. glass thickness 
                                  3. the characteristic of PDLC film. 
                                Therefore, trial and test is required to obtain 
                                  the most optimum procedure and data. 
                                The temperature mentioned above always refers 
                                  to glass surface temperature. 
                                  |