Production technology  | 
                             
                             
                              |   | 
                             
                             
                               | 
                             
                             
                              |   | 
                             
                             
                              It is the high-tech product 
                                  that our company developed newly that the environmental 
                                  protection type glass is powder for glass etching 
                                  by chemical; it adopts the running water to 
                                  prepare the liquid. To plate glass, daily glass, 
                                  lamp decoration glass, etc. can product the 
                                  product result well, it is high-efficient, environmental 
                                  protection, security, such advantages as easy 
                                  to operate, each kilogram powder can deal with 
                                  15M2(count with the form).  
                                Liquid preparation 
                                This kind of powder pairs of 
                                  group copies of product, each packaging include 
                                  A group a copy of 17.5 kilograms, group B is 
                                  a piece of 7.5 kilograms. While preparing and 
                                  is covered with the sand liquid, a piece of 
                                  7 according to group A, group B is a piece of 
                                  3, the proportion of adding 3 pieces of running 
                                  water is prepared, concrete can consult the 
                                  proportion of the form. 
                                     | 
                             
                             
                              |   | 
                             
                             
                              |  Unit: kgs | 
                             
                             
                               
                                   
                                    | Material A | 
                                    0.7 | 
                                    1.4 | 
                                    3.5 | 
                                    7 | 
                                    14 | 
                                    17.5 | 
                                   
                                   
                                    | Material B | 
                                    0.3 | 
                                    0.6 | 
                                    1.5 | 
                                    3 | 
                                    6 | 
                                    7.5 | 
                                   
                                   
                                    | Running water | 
                                    0.3 | 
                                    0.6 | 
                                    1.5 | 
                                    3 | 
                                    6 | 
                                    7.5 | 
                                   
                                  | 
                             
                             
                              |   | 
                             
                             
                              | Put plastic barrel with B group 
                                copy A group copy pro rata first when preparing, 
                                add running water pro rata and then (prepare with 
                                more than 80℃ hot water, can shorten familiar 
                                to take time over half), use plastics (or bamboo, 
                                wood) excellent to mix to even fully, prepare 
                                liquid medicine well is it seal to cover properly, 
                                let it naturally familiar to take for 24 hours 
                                under room temperature. Prepare newly powder to 
                                be liquid relatively thick, temperature drop, 
                                after slaking liquid medicine viscidity, temperature 
                                can return to normal. The compounding amount should 
                                lengthen the familiar time of melting properly 
                                greatly and when it is colder).   Process 
                                 
                                Prepared liquid fully mixed first, the solid 
                                  depositing in the container bottom must be stirred, 
                                  the liquid of suspending until forming a state, 
                                  is and then soaked the clean glass products 
                                  in the liquid, quiet to put one about 2 minutes, 
                                  is it liquid flow back to the barrel to make 
                                  while being about 5-10 seconds to take out. 
                                  Using temperature to keep among 10-35℃ of liquid. 
                                 Washing and Drying 
                                 
                                Let through processed glass products wash or 
                                  clean spray with running water have to undergo, 
                                  can also develop with the running water after 
                                  scrubbing with the soft cloth, the glass products 
                                  after cleaning can be dried or dried naturally. 
                                 Usage and maintenance 
                                  of the prepared liquid 
                                 
                                1. Is it confirming person who adds to come 
                                  according to amount of production, produce 200M2 
                                  about glass each time (basis on single side 
                                  process), need to add a case of powder. Confirm 
                                  the way of adding according to the surface of 
                                  pool liquid while adding: If it is high enough 
                                  the liquid, add to the pool directly (produce 
                                  the post addition at that night), fetch liquid 
                                  is it turn on to come, pour into pool after 
                                  melt familiarly well, if liquid high enough 
                                  in pool, adding the concentrate, the concentrate 
                                  is prepared as follows: 1 case powder +5 kilograms 
                                  water (best for hot water) or 1 case powder 
                                  +5 kilograms old liquid, for is it is it had 
                                  better turn on kind concentrate for future spending 
                                  first with container to produce in succession 
                                  to guarantee, It treats to be enough high efficacy 
                                  of a drug is it put pool into to mend when reducing 
                                  , need time to be familiar to take like this 
                                  the liquid, thus avoid stopping production. 
                                  If produced according to the above method strictly, 
                                  is the prepared liquid and can be guaranteed 
                                  to use normally.  
                                2. Because operate improper or other reasons, 
                                  may cause the prepared liquid and present the 
                                  following problems, 
                                ①The surface of processed glass, have mark 
                                  of spending (namely not the so-called and dirty), 
                                  the liquid the sour and on the high side for 
                                  sand mainly (the getting on the high more side 
                                  definitely on the high side in powder) cause, 
                                  cause the reason as follows: The prepared liquid 
                                  is it stand up to stir fully, bottom is it powder 
                                  in a large amount to deposit, is it on the low 
                                  side powder in the liquid to cause, the acid 
                                  is relatively on the high side. Solution: Mix 
                                  precipitating and disperse it evenly in cheating 
                                  the sand liquid. 
                                ②It is effectual to be processed but time is 
                                  long; this is mainly a cause of acid on the 
                                  high side. Solution: Regulating hydrogen PH 
                                  among 2-3 through adding the dense sulfuric 
                                  acid, it is 2.5 to be the best, can't be smaller 
                                  than 2. Add the method: Generally every 25 kilograms 
                                  are covered with sand powder and added 0. 5-1 
                                  kilograms of dense sulfuric acids, is 0 with 
                                  the volume of the tank. 4-0. 8M3; come it count, 
                                  need it for 14-28 kilograms. Add the step: Add 
                                  14 kilograms of dense sulfuric acids and mix 
                                  and is prepared liquid evenly first, examine 
                                  hydrogen PH, if already on the normal range, 
                                  stop adding, on the contrary, add 2 kilograms 
                                  of dense sulfuric acids each time according 
                                  to this method again, until PH being on the 
                                  normal range. 
                                ③The glass surface is very difficult to dust 
                                  or be totally covered with the sand, it is possible 
                                  as follows,  
                                a. The acid is too low; PH is greater than 
                                  more than 4. Press ② Method it can be solve 
                                  it. 
                                  b. The acid is in normal, the getting less too 
                                  in powder. Add and powder in a large amount, 
                                  make it look thick enough to liquid. (Whether 
                                  can with newly opened liquid contrast, should 
                                  have more brilliant form thing among liquid 
                                  generally) 
                                  c. Sour and all scarce powder, covered with 
                                  the sand liquid and looked like the white milk 
                                  form, can not see the brilliant form thing. 
                                  Solution: Is it powder in a large amount to 
                                  add, is it adds strong sulfuric acid to complement, 
                                  is it covers with consistency and acidity, liquid 
                                  all on the normal range to make. The adding 
                                  amount of dense sulfuric acid is generally complemented 
                                  with 0 for every case powder. 5-1 kilograms. 
                                 Packaging and 
                                  quality guarantee period 
                                 
                                Packaging: 25 kilograms of cartons pack the 
                                  damp proof plastic bag of inside lining. (Include 
                                  A group copies of 17 inside. 5 kilograms; one 
                                  of group B is 7. 5 kilograms) 
                                Quality guarantee period: Two years 
                                 
                                 | 
                             
                           
                           | 
                       
                    
                    |